The B400 handheld oxygen cutting torch is suitable for extended work. Its dual-tube design allows for a cutting depth of up to 300mm. Its high-quality forged brass head provides enhanced durability. Available acetylene cutting nozzles: 1502mm. Available propane cutting nozzles: 1503mm.
| Specification Category | English Description |
| Compatible Gases | Acetylene, propane |
| Cutting Capacity | Up to 300mm |
| Compatible Cutting Nozzles | Acetylene gas: 1502; Propane gas: 1503 |
The B400 Heavy-Duty Handheld Oxygen Acetylene Cutting Torch is engineered for maximum performance and durability in demanding industrial environments. Built with a high-quality forged brass head, it offers exceptional strength, resistance to heat and wear, and a longer service life. Its dual-tube design ensures stable gas flow and enhanced cutting efficiency, allowing for clean, precise cuts with outstanding control. With an impressive cutting capacity of up to 300mm, the B400 is capable of handling even the toughest metal cutting tasks. It is equipped with Acetylene cutting nozzle 1502 and Propane cutting nozzle 1503, giving users the flexibility to choose their preferred fuel type. Designed for heavy-duty applications such as construction, shipbuilding, steel fabrication, and repair work, the B400 provides reliable performance, safety, and precision every time.
A welder picks up a torch with a size-2 tip, lights it, sets what looks like a neutral flame, and still finishes the shift with a cut edge that needs grinding and a bead that crac...
READ MOREThree faults account for most poor oxy acetylene cuts: a tip that is too large for the plate, regulator pressures set by memory instead of by a chart, and a connection that leaks ...
READ MOREA cutting torch that pops at the tip, a kerf that drifts to one side, a tip that keeps fusing itself to the plate — these faults usually start nowhere near where they show up. The...
READ MOREA #1 tip, roughly 28 psi of oxygen and 4 psi of acetylene will take a 6 mm mild steel plate apart in a few seconds. Run the same torch onto 25 mm plate without touching anything a...
READ MOREA clean oxy-acetylene cut is mostly a matter of order and numbers. Inspect the outfit, set each regulator to the pressure chart for the tip in the torch, purge both hoses, light t...
READ MORE