The 1-101 Series Acetylene Torch Tips – your go-to solution for precision, power, and reliability in industrial cutting applications. Specifically engineered for use with acetylene gas, these high-performance tips deliver a clean, concentrated flame that ensures smooth, efficient cuts every time. With a standardized 76mm length, they’re designed for optimal heat control and easy handling, making them ideal for both seasoned professionals and skilled tradespeople. The 1-101 series is fully compatible with a wide range of popular torches, including models A217, A218, A219, A246, A212, and A800—offering seamless integration into your existing setup without the need for adapters or modifications. Whether you’re cutting thin sheet metal or tackling thick steel plates up to 200mm, these tips provide consistent performance across a broad cutting range of 5–200mm. Trusted in fabrication shops, shipyards, and construction sites worldwide, the 1-101 Series combines durability with precision to help you get the job done faster and cleaner. Upgrade your cutting operation today with tips built for real-world demands and unmatched versatility.
| Name | Model | Gas | Applicable cutting torch | cutting thickness | Oxygen pressure | Gas pressure | Cutting length(mm) |
| 1-101 Series | 1-1-101 | Acetylene | A217,A218,A219,A246,A212,A800 | 5-10MM | 1.5bar | 0.5bar | 76MM |
| 1-1-101 | 10-30MM | 2.0bar | 0.5bar | ||||
| 3-1-101 | 30-50MM | 2.0bar | 1.0bar | ||||
| 4-1-101 | 50-70MM | 2.5bar | 1.0bar | ||||
| 5-1-101 | 70-150MM | 3.0bar | 1.5bar | ||||
| 6-1-101 | 150-200MM | 3.5bar | 1.5bar |
A clean oxy-acetylene cut is mostly a matter of order and numbers. Inspect the outfit, set each regulator to the pressure chart for the tip in the torch, purge both hoses, light t...
READ MOREA fabricator preparing to cut 25 mm steel plate has a practical question: how hot is an acetylene torch? The useful answer is about 3,150 to 3,330°C (5,700 to 6,030°F) when acetyl...
READ MOREA properly adjusted oxy-acetylene torch produces a neutral flame of about 3,300°C (6,000°F) at the tip of the inner cone, and normal working values stay in the 3,100–3,300°C (5,60...
READ MORELight a properly adjusted oxy-acetylene torch and the tip of the inner cone sits somewhere between 5,600°F and 6,300°F (3,100–3,480°C). That makes acetylene, when burned with pure...
READ MOREYour workstation needs a gas cutting torch, but the moment you start comparing models, the specs stop making sense. Every supplier calls its product heavy duty, yet the handles we...
READ MORE