ACETYLENE


Tip2890-1F2890-2F2890-3F2890-4F2890-5F2890-6F

CuttingThickness  

(mm)

0-1010-5050-100100-125125-150150-200
Oxy.Pressure(Bar)1.0-1.51.5-2.53.0-4.55.0-5.55.5-6.06.0-6.5
Ace./Pro.Pressure(Bar)0.20.30.50.70.70.7

Lenglh

(mm)

787878787878