ACETYLENE


Tip6290-000AC6290-00AC6290-0AC6290-1AC6290-2AC6290-3AC6290-4AC6290-5AC6290-6AC

CuttingThickness  

(mm)

1-55-1010-1515-2525-5050-100100-175175-250250-300
Oxy.Pressure(Bar)1.51.52.02.53.03.54.05.06.0
Ace./Pro.Pressure(Bar)0.50.51.01.01.01.01.51.51.5

Lenglh

(mm)

535353535353535353