PRODUCT DETAILS

ANME

ACETYLENE


TipANME-1 (1/32")ANME-2 (3/64")ANME-3 (1/16")ANME-4 (5/64")ANME-5 (3/32")ANME-6 (7/64")ANME-7 (1/8")
Cutting Thickness (mm)3-1010-2525-4040-6060-100100-200200-300
Oxy. Pressure(Bar)2.5-3.53.0-4.03.5-4.54.5-5.04.5-5.55.0-6.56.0-7.5
Ace.Pressure(Bar)0.30.30.30.50.50.50.8
Length(mm)88888888888888